From: Electro-capacitive performance of haemoglobin/polypyrrole composites for high power density electrode
S.No.
Name of materials
Electrolyte
Cs(F/g)
Current density (mA/cm2)
Energy density (Wh/Kg)
Power density (W/Kg)
1
PPy
1.0 M KOH
200.56
10
6.26
259.76
2
HPyC3%
445.75
14.37
596.54